Synthesis and Luminescence Properties of Pure and Doped with Europium(III) K0.45Bi0.55Mo0.9V0.1O4 Solid Solutions |
V.P. Chorniia, b, V.V. Boykoa, S.G. Nedilkob, O.V. Petrenkob, V.M. Prokopetsb, K.V. Terebilenkob, M.S. Slobodyanykb
aNational University of Life and Environmental Sciences of Ukraine, 15 Geroiv Oborony str., 03041 Kyiv, Ukraine bTaras Shevchenko National University of Kyiv, 64/13 Volodymyrska str., 01301 Kyiv, Ukraine |
Full Text PDF |
The results of synthesis, crystal structure characterization, and luminescence properties study of pure and Eu3+-doped K0.45Bi0.55Mo0.9V0.1O4 solid solutions have been reported. The obtained powders crystallize in a compact form with an average size of the particles of about 5-10 μm. It was found that doping with europium leads to the transformation of the host from monoclinic to tetragonal scheelite-like phase. The Eu3+-doped samples reveal intensive red luminescence under excitation in ultraviolet and blue spectral regions. Energy transfer from molybdate-vanadate host to Eu3+ ions takes place in the studied solid-solution. Intensity of the red luminescence increases when Eu3+ content increases and no concentration quenching has been found. |
DOI:10.12693/APhysPolA.141.237 topics: bismuth, europium, luminescence, molybdate |