Influence of Vitroperm Content on the Energy Losses in Composite Materials Based on the Mixture of Two Ferromagnets
Z. Birčákováa, P. Kollára, V. Vojteka, R. Burešb, M. Fáberováb
aInstitute of Physics, Faculty of Sciences, P. J. Šafárik University, Park Angelinum 9, 041 54 Košice, Slovakia
bInstitute of Materials Research SAS, 040 01 Košice, Watsonova 47, 040 01 Košice, Slovakia
Full Text PDF
Soft magnetic composites offer several advantages such as 3D isotropic magnetic properties and relatively small energy losses, finding use in electrical devices like electromotors, transformers or sensors. The aim of this work was to investigate the dc and ac magnetic properties of composites based on the mixture of two different ferromagnets: iron based material Somaloy® 700 and Vitroperm® 500 alloy. The analysis of total losses into dc losses, classical losses and excess losses showed that the classical and excess losses were negligibly small. The specific resistivity was increasing with the increasing fraction of Vitroperm (VPM). The coercivity exhibited maximum at 20% of VPM.

DOI: 10.12693/APhysPolA.126.114