Soft Magnetic Properties in Bulk Permalloy Alloys Fabricated by a Warm Consolidation
J. Fűzer a, P. Kollár a, D. Olekšáková b and S. Roth c
a Institute of Physics, Faculty of Sciences, P.J. Šafárik University, Park Angelinum 9, 04154 Košice, Slovakia
b Department of Applied Mathematics, Faculty of Mechanical Engineering, Technical University in Košice, Letná 9, 04200 Košice, Slovakia
c IFW Dresden, Helmholtzstr. 20, Postfach 270016, 01069, Dresden, Germany
Full Text PDF
Received: 9 07 2007;
Soft magnetic properties of bulk NiFe and NiFeMo alloys consolidated by hot compaction were studied. During annealing the compacts residual stresses diminish by relaxation and soft magnetic properties improve. The lowest coercivity of bulk NiFe and NiFeMo alloys are 11.0 and 11.2 A/m, respectively, while the total losses are 1.81 and 1.42 W/g at f=10 kHz and Bmax=0.2T.
DOI: 10.12693/APhysPolA.113.59